i'm forming pipes into bends by heat induction coil , how can i keep the yield and tensile of the pipes after
Jul 16, 2006 by ahmed_hashash | Posted in Engineering
i'm forming high grades carbon steel pipes into bends ( elbows) using induction hot coils , i don't know how to maintain the yield and tensile strenght because everytime after bending the test result of the bent area illustrate lower grade. any suggestions???
You've got a bit of a problem.
Let's say you were using 0.30% carbon tubing that was heat treated to a certain tensile and yield strength. In order for the original tubing to be hardened, it had to be heated to the austenitic temperature
jimdempster | Jul 17, 2006
What's hot
Peerless 5630448 Grade 43 Low Carbon Steel High Test Industrial Coil Chain in Half Drum, Hot Galvanized, 3/8" Trade, 0.392" Wire Diameter, 200' Length, 5400 lbs Load Capacity BISS (Peerless)
Price: $263.54
Heavy duty trucking, farm and construction firms
Hot galvanized finish
Working load limits exceed those of ordinary low carbon or general utility chain
Peerless 8610219 Grade 43 Carbon Steel High Test Tiedown Coil Chain Assembly, Self Colored, 20' Length, 2600 lbs Load Capacity BISS (Peerless)
Price: $74.66
Self colored finish
Comes in standard pack
Working load limits exceed those of ordinary low carbon or general utility chain